{"pub_number":"JPH08321010A","doc_number":"H08321010","country":"JP","kind_code":"A","patent_type":"utility","status":"expired","title":"Thin film magnetic head","abstract_text":"PURPOSE: To obtain a thin film magnetic head with a CoNiFe film excellent in soft magnetic characteristics and corrosion resistance. CONSTITUTION: When a magnetic film is formed on a substrate 1 by electroplating, a CoNiFe film having a compsn. consisting of 74wt.% Co, 21wt.% Ni and 5wt.% Fe is formed in 15nm average grain size by forming a film at 40nm/sec plating rate which is lower than the conventional rate. The CoNiFe film has 20e coercive force, a magnetostriction of 2×10&lt;-6&gt; and -0.08V corrosion potential to NiFe and is excellent in corrosion resistance.","claims":[],"description":"","inventors":[{"name":"Komaki Kenji","slug":"komaki-kenji"},{"name":"Suzuki Koichi","slug":"suzuki-koichi"}],"assignees":[{"name":"Sumitomo Metal Ind","slug":"sumitomo-metal-ind"}],"examiners":[],"cpc_codes":[],"ipc_codes":["C22C 19/00","C23C 14/00","G11B 5/127","G11B 5/31"],"filing_date":"1995-05-26","pub_date":"1996-12-03","priority_date":"1995-05-26","expiration_date":"2015-05-26","application_number":"JP-12829995-A","family_id":"FAM-14981366","family_members":[],"citations_made":[],"non_patent_literature":[],"drawings_count":0,"source_id":"google_patents_public","upstream_forward_citations":0,"metrics":{"forward_citations":5,"indexed_forward_citations":5,"backward_citations":0,"npl_citations":0,"citations_per_year":0.17,"pagerank":1.8999803066253664,"citation_rank":19649503,"pagerank_rank":15771706,"velocity_rank":36018444,"family_citations":5}}