{"pub_number":"JP2005294438A","doc_number":"2005294438","country":"JP","kind_code":"A","patent_type":"utility","status":"expired","title":"Thermal oxidation method, piezoelectric actuator with substrate formed thereby, and liquid injection device","abstract_text":"&lt;P&gt;PROBLEM TO BE SOLVED: To provide a thermal oxidation method in order to stabilize the adhesion of a metallic oxide film and an underlying layer. &lt;P&gt;SOLUTION: The thermal oxidation method is performed such that two or more substrates 14 are fixed to a jig 12, and supplied to a thermal oxidation furnace 10, in order to form a metallic oxide film by oxidizing the metal film on the surface of a substrate. The distance between the substrates fixed to the jig is set at least 1/4 or more of the substrate diameter. The metal film comprises one of zirconium, aluminum, and titanium. It is preferable that the transfer speed is preferably 200 mm/minute or more at the time of supplying the jig to the thermal oxidation furnace. &lt;P&gt;COPYRIGHT: (C)2006,JPO&amp;NCIPI","claims":[],"description":"","inventors":[{"name":"Murai Masami","slug":"murai-masami"},{"name":"Ito Maki","slug":"ito-maki"}],"assignees":[{"name":"Seiko Epson Corp","slug":"seiko-epson-corp"}],"examiners":[],"cpc_codes":[],"ipc_codes":["B05C 5/00","B41J 2/14","B41J 2/145","B41J 2/16","H10N 30/01","H10N 30/20","H10N 30/853"],"filing_date":"2004-03-31","pub_date":"2005-10-20","priority_date":"2004-03-31","expiration_date":"2024-03-31","application_number":"JP-2004105641-A","family_id":"FAM-35327053","family_members":[],"citations_made":[],"non_patent_literature":[],"drawings_count":0,"source_id":"google_patents_public","upstream_forward_citations":0,"metrics":{"forward_citations":6,"indexed_forward_citations":6,"backward_citations":0,"npl_citations":0,"citations_per_year":0.29,"pagerank":1.5764654874801636,"citation_rank":17889614,"pagerank_rank":21167714,"velocity_rank":26155333,"family_citations":6}}