{"pub_number":"JP2001240407A","doc_number":"2001240407","country":"JP","kind_code":"A","patent_type":"utility","status":"expired","title":"Activated carbon and its manufacturing method","abstract_text":"PROBLEM TO BE SOLVED: To provide an activated carbon capable of adsorbing small molecular weight materials efficiently and its manufacturing method. SOLUTION: The pore diameter of the activated carbon is uniform, the specific surface area is 500-3,000 m2/g and the adsorption quantity of nitrogen is 10 ml/g or more at 25 deg.C and 1 atmospheric pressure. The activated carbon is manufactured by the activation of a carbon material at 600-1,200 deg.C under an atmosphere that contains carbon dioxide as the main component, 2 vol.% or less steam and 2 vol.% or more carbon monoxide.","claims":[],"description":"","inventors":[{"name":"Abe Susumu","slug":"abe-susumu"},{"name":"Ishimura Shizuo","slug":"ishimura-shizuo"}],"assignees":[{"name":"Kuraray Chemical Kk","slug":"kuraray-chemical-kk"}],"examiners":[],"cpc_codes":[],"ipc_codes":["B01J 20/20","C01B 32/336"],"filing_date":"2000-11-14","pub_date":"2001-09-04","priority_date":"1999-12-24","expiration_date":"2020-11-14","application_number":"JP-2000346693-A","family_id":"FAM-26581707","family_members":[],"citations_made":[],"non_patent_literature":[],"drawings_count":0,"source_id":"google_patents_public","upstream_forward_citations":0,"metrics":{"forward_citations":40,"indexed_forward_citations":40,"backward_citations":0,"npl_citations":0,"citations_per_year":1.6,"pagerank":11.767256736755373,"citation_rank":1373607,"pagerank_rank":810319,"velocity_rank":3090921,"family_citations":40}}