{"pub_number":"EP1069241B1","doc_number":"1069241","country":"EP","kind_code":"B1","patent_type":"utility","status":"expired","title":"Method for producing a surfacing and groundcovering","abstract_text":"The covering material consists of a mixture of a bitumen binder (4) and crushed rock (1, 5) with the binder having a density greater than that of the rock. The rock particles are preferably 2 - 18 mm in size and comprise between 25 and 55 per cent of the mixture&#39;s mass. After laying, the surface of the layer is ground, e.g. by diamond plates, and then cleaned with rotary plastic brushes and water to leave the surface rock particles exposed. The resultant slurry is removed by suction.","claims":[],"description":"","inventors":[{"name":"Bony Bruno","slug":"bony-bruno","country":"FR"}],"assignees":[{"name":"Asten","slug":"asten","country":"FR"}],"examiners":[],"cpc_codes":["E01C 11/24","E01C 7/182"],"ipc_codes":["E01C 11/24","E01C 7/18"],"filing_date":"2000-07-12","pub_date":"2004-06-16","grant_date":"2004-06-16","priority_date":"1999-07-16","expiration_date":"2020-07-12","application_number":"EP-00402014-A","family_id":"FAM-9548214","family_members":[],"citations_made":[],"non_patent_literature":[],"drawings_count":0,"source_id":"google_patents_public","upstream_forward_citations":0,"metrics":{"forward_citations":1,"indexed_forward_citations":1,"backward_citations":0,"npl_citations":0,"citations_per_year":0.05,"pagerank":0.7488889098167419,"citation_rank":61372870,"pagerank_rank":61372870,"velocity_rank":54889128,"family_citations":1}}